1. Material Performance Requirements
1.1 Base Plate Material
316L stainless steel (standard type)
Chemical composition meets ASTM A240 / EN 1.4404
Low carbon (C ≤ 0.03%) to prevent intergranular corrosion
Mo ≥ 2.0% for strong pitting resistance in acidic electrolyte
Duplex stainless steel (high‑strength type: 2205 / LDX 2101)
Austenite + ferrite dual‑phase structure
Yield strength ≥ 450 MPa (double that of 316L)
PREN ≥ 28 for high chloride resistance
No stress corrosion cracking (SCC)
1.2 Conductive Beam Material
Copper‑clad steel (CCS)
Copper layer thickness: 1.0–3.0 mm
Bonding strength: no peeling, no bubbling, no cracking
Or copper core composite structure
Surface conductivity ≥ 97% IACS
1.3 Edge & Sealing Materials
EDGE strips: high‑quality PVC / PP / rubber
High temperature resistance: 70°C
Acid resistance: sulfuric acid 10%–20%
No deformation, no falling off
2. Dimensional Accuracy & Flatness Requirements
The most important indicator to avoid short circuits
2.1 Overall Dimensions
Length, width, thickness tolerance: ± 0.5 mm
Diagonal difference ≤ 1.0 mm
Consistent size for all plates
2.2 Flatness
Flatness ≤ 1.0 mm/m
Overall warpage ≤ 2 mm for the full plate
No bending, twisting, or bulging
Ensures uniform anode–cathode gap
2.3 Parallelism & Perpendicularity
Beam and plate perpendicularity error ≤ 0.5 mm
Parallelism between two sides ≤ 0.5 mm
Ensures smooth operation in automatic stripping machines
3. Welding Performance Requirements
3.1 Welding Method
Automatic submerged arc welding or laser welding
Full penetration, no lack of fusion, no porosity, no cracks
3.2 Weld Strength
Weld strength ≥ base metal strength
No fracture under lifting, stripping, and handling
3.3 Weld Corrosion Resistance
Weld zone must not corrode earlier than base plate
Passivation treatment after welding
100% appearance inspection + optional NDT
3.4 Conductive Beam Welding
Weld continuity
Low contact resistance
No virtual welding (critical for conductivity)
4. Electrical Performance Requirements
4.1 Contact Resistance
Conductive beam contact resistance ≤ 50 microohms (μΩ)
High‑grade design ≤ 20 μΩ
Directly affects power consumption of the whole refinery
4.4 Voltage Drop
Overall voltage drop ≤ 5 mV under working current
Reduces power waste
4.3 Current Distribution Uniformity
Surface current density deviation ≤ 5%
Ensures uniform copper deposition
No nodules, no rough edges
5. Surface Quality Requirements
5.1 Surface Roughness
Ra ≤ 0.8 μm
Smooth surface for easy stripping
No copper adhesion
5.2 Surface Defects
No scratches, bumps, pits, or oxide scales
No mechanical damage
No rust or color difference
5.3 Passivation & Protection
Electropolishing or chemical passivation
Improve corrosion resistance
Improve stripping performance
6. Corrosion Resistance Requirements
For copper electrolyte (H₂SO₄ + CuSO₄ + Cl⁻)
6.1 Pitting Corrosion Resistance
No pitting in 60°C acidic electrolyte for 12 months
316L used for low chloride
Duplex used for high chloride
6.2 Crevice Corrosion Resistance
No crevice corrosion at beam welds
No corrosion at edge strips
6.3 Stress Corrosion Resistance
Duplex stainless steel: no SCC
Suitable for high temperature & high chloride
6.4 Service Life
316L: 8–12 years
Duplex: 12–15+ years
7. Mechanical Strength & Rigidity Requirements
7.1 Structural Strength
No deformation during long‑term vertical hanging
No bending under 100–150 kg copper sheet load
7.2 Rigidity
High resistance to warping
Maintains shape in automatic handling
7.3 Impact Resistance
Resists impact during stripping and transport
No cracks, no deformation
8. Stripping Performance Requirements
8.1 Easy Stripping
Copper sheet can be completely stripped in one time
No sticking, no tearing
No copper residue on stainless steel surface
8.2 No Edge Growth
Edge strips effectively block copper overgrowth
Ensure neat cathode edges
8.3 Adaptability to Automatic Stripping Machines
Fully compatible with ISA / KIDD / OK automatic stripping systems
High pass rate ≥ 99.5%
9. Thermal Stability Requirements
Working temperature: 45–65°C
No thermal deformation
No thermal aging of edge materials
No warping at high temperature
10. Comprehensive Service Life & Reliability
Average service life ≥ 10 years
Damage rate ≤ 0.5% per year
Maintenance cost extremely low
High operational stability
Final Summary: All Key Performance Requirements (For Technical Specification)
Material: 316L or duplex stainless steel, copper‑clad beam
Dimension tolerance: ±0.5 mm
Flatness: ≤1 mm/m
Weld: full penetration, high strength, corrosion resistant
Contact resistance: ≤50 μΩ
Surface roughness: Ra ≤0.8 μm
Corrosion resistance: no pitting, no crevice corrosion, no SCC
Mechanical rigidity: no deformation, no bending
Stripping performance: easy stripping, no adhesion
Service life: 8–15 years